Hello all,

I am looking for a non-conductive fiberglass tube.

this tube needs to be approx. 7/16" OD by 5/16" ID..and it needs to be able to withstand 2000 psi of hydraulic oil..

I have been looking everywhere locally and no one carries this stuff..

any help would be appreciated..

thanks,
brent
 
Replies continue below

Recommended for you

I've used FRP tube in larger sizes, and found that you had to pay extra to get a good surface finish on the outside ... and that surface was cosmetically very nice, but not uniform enough to use with an o-ring.