HI,
1) Whenever it rains fiber cement siding in my house starts to wrinkle as shown in the image 1. Once the sun comes out it dries up and all the wrinkles goes away. Is this just the paint on the cladding giving away? Why is this happening? Is this something I need to be concerned about? Any structural issue? There is no water stains/leaks on the inside the house on the walls at this location.
2) Image 2 is of one of the room ceilings. I see like a bulge on the ceilings at various spots. What are these spots? Is it because of ceiling not finished well? Any structural concerns with this?
1) Whenever it rains fiber cement siding in my house starts to wrinkle as shown in the image 1. Once the sun comes out it dries up and all the wrinkles goes away. Is this just the paint on the cladding giving away? Why is this happening? Is this something I need to be concerned about? Any structural issue? There is no water stains/leaks on the inside the house on the walls at this location.
2) Image 2 is of one of the room ceilings. I see like a bulge on the ceilings at various spots. What are these spots? Is it because of ceiling not finished well? Any structural concerns with this?