My understanding about Duplex S.S is mostly used in pressure vessels. Ferrite content testing is important quality test for its welding because mostly it has to perform in corrosive environment with high thermal stresses.
But,we are using Duplex SS (EN std. 1.4462)in rolling stock underframe where the environment is not highly corrosive and stresses are present due to static/ dynamic loading only.
Can anybody suggest what is the relevance of ferrite tests done on Duplex SS welds for application in structures.
But,we are using Duplex SS (EN std. 1.4462)in rolling stock underframe where the environment is not highly corrosive and stresses are present due to static/ dynamic loading only.
Can anybody suggest what is the relevance of ferrite tests done on Duplex SS welds for application in structures.