ferrite number

Status
Not open for further replies.

lahane1443

Mechanical
Oct 12, 2010
50
I have a weld procedure for austenitic steel with solution annealing. now there is a requirement of ferrite Number of weld metal. Can I weld a test sample only to conduct Ferrite Number test on weld metal using the same consumable brand as that was used for PQR and add as a addenda to PQR?
 