Hello,
I would like to ask you if the non homogeneous area with bids is normal in ferrite core manufacturing or it is a manufacturing defect:
We have and issue of increased noise generation with this type of core from a certain supplier and I am curious if this could have effect on the problem.
Gabriel.
I would like to ask you if the non homogeneous area with bids is normal in ferrite core manufacturing or it is a manufacturing defect:
We have and issue of increased noise generation with this type of core from a certain supplier and I am curious if this could have effect on the problem.
Gabriel.