SJones
Petroleum
- Apr 22, 2001
- 3,931
NORSOK M-605 requires an ASTM G48 method A test, 50 deg C 24 hours, for ASTM A494 castings in N06625 but not for pipe, tube, forgings, fittings etc. The acceptance criteria are the same as for austenitic alloys: No pitting at x20 magnification and max weight loss of 4g/m2.
Q1. Why only test castings?
Q2. Is a G48 A test for N06625 and N08825 of any value as a production quality control test for all product forms used in piping systems?
Q3. If they are of any use, is it valid to adopt the same criteria as for austenitic and duplex alloys?
Steve Jones
Materials & Corrosion Engineer
Q1. Why only test castings?
Q2. Is a G48 A test for N06625 and N08825 of any value as a production quality control test for all product forms used in piping systems?
Q3. If they are of any use, is it valid to adopt the same criteria as for austenitic and duplex alloys?
Steve Jones
Materials & Corrosion Engineer