I work in a company that produces a product that is used by the the military. The process is very much like powdered metal pressing. Instead of metal powder we are pressing very reactive mixtures of powders to make a solid material. The problem is that our feed shoes are experencing extreme amounts of wear. We have tried several types of plastics (UHMV, Poly). One other problem is foreign objects, shoe material and organic material in our pressed item causes very noticable effects on performance, so in Xray inspection we have a reject products with FO.
My next shoe material is going to be anodize aluminum. Any other sugestions to a shoe bottom that i should try?I am also looking to get input on changing out our current automatic feed shoe design.
My next shoe material is going to be anodize aluminum. Any other sugestions to a shoe bottom that i should try?I am also looking to get input on changing out our current automatic feed shoe design.