In looking at stresses on a plastic material in FEA, do you use the von mises or max principal as your stress criteria?
 
Replies continue below

Recommended for you

Do you mean plastic in the sense of an organic material, or do you mean a material in a plastic condition ? If its the former, and exhibits brittle failure, I would say Max. Principal. If it exhibits ductile failure, I would say Von Mises. Both types of failure can occur with plastics, but don't ask me which ones occur with which materials and conditions of loading.
 
Suggest you post in an FEA Forum. There are several.
 