Hello greetings to everyone,
I am trying to model hydrostatic testing to destruction of some Ductile Iron castings. All castings have some defects. But my FEA model does not model these defects. My question is: How much discrepency should one expect in the predicted burst pressrue because of this discrepency?
Thanks
Gurmeet
I am trying to model hydrostatic testing to destruction of some Ductile Iron castings. All castings have some defects. But my FEA model does not model these defects. My question is: How much discrepency should one expect in the predicted burst pressrue because of this discrepency?