SMontgomery119
Mechanical
- Nov 30, 2007
- 11
Hello,
I am looking for FEA software to help model a pipe-to-vessel interface.
As displayed in the attached drawing, the pipe has two 90-degree bends shortly before interfacing the pressure vessel. The pipe/vessel interface is supported with a 24"x24" and 3/16" thick plate. The piping fluid temp. variation is 95 to 400-degree F.
The problem is a recurring weld failure at the pipe/plate interface.
Any fea software suggestions to redesign the pipe-to-vessel interface?
Below are some packages I've found:
Chempute - nozzle pro
Algor - pipepak
Codeware - nozzle pro
Are there other suitable fea programs?
Thanks,
Steve M.
I am looking for FEA software to help model a pipe-to-vessel interface.
As displayed in the attached drawing, the pipe has two 90-degree bends shortly before interfacing the pressure vessel. The pipe/vessel interface is supported with a 24"x24" and 3/16" thick plate. The piping fluid temp. variation is 95 to 400-degree F.
The problem is a recurring weld failure at the pipe/plate interface.
Any fea software suggestions to redesign the pipe-to-vessel interface?
Below are some packages I've found:
Chempute - nozzle pro
Algor - pipepak
Codeware - nozzle pro
Are there other suitable fea programs?
Thanks,
Steve M.