Fatigue properties for an alloy similar to VACOFLUX 9CR

Status
Not open for further replies.

kevlar49

Materials
Joined
Jun 1, 2006
Messages
287
Location
US
We are using this alloy called VACOFLUX 9CR. Unfortunately, the manufacturer does not have fatigue characterization of it. Does anyone know of a similar alloy that may have fatigue data associated with it?
 
Check with VAC. If they do not have the data, i doubt everyone else has. This a very unique magnetic grade. I am not aware anyone other than VAC is making it, not even a similar alloy.
Also, you need to specify condition fro fatigue, e.g. full anneal at magnetic optimized condition, or mill annealed, or cold worked with xx% cold reduction etc.
 