AISC Table A-3.1 Item 2.3 is listed as "Base metal at the net section of other mechanically fastened joints except eye bars and pin plates. The illustration adds (Note: figures are for snug-tightened bolts, rivets, or other mechanical fasteners.) There is nothing in this listing that either specifically permits or excludes a mild steel bolt. Stress Category D
Constant Cf 22 x 10^8
Threshold Fth ksi (MPa) 7 (48)
Potential Crack Initiation Point "In net section originating at side of hole"
With the exception of Table J3.2 that shows the nominal strength of various fasteners, an ASTM A307 mild steel bolt is not mentioned within the AISC Specification.