I'm looking for fatigue life data on Kel-F (actually now called Neoflon and made by Daikin). Any graded is fine, M-300 or M-400. I'll be making some machined parts (not molded) that are under significant cyclical stress and would like to design for infinite life.

Thanks,
Dave.
 
Replies continue below

Recommended for you

I have no data on this one.

I guess you tried the manufacturer.

If you do get figures for moulded parts, you will get a different result from machined parts. It might be significantly different as there are a fer variables involved

Regards
pat