APRRK...
I have a copy of a ~20-YO ASMH Hdbk. The examples listed are not full extent of data for H1150 fatigue data. I am not comfortable copying/pasting that data [SN figures], here.
NOTE.
Several years ago the ASMH was handed-over to industry for maintenance and updates.... and has been renamed as Aerospace Structural Metals Database. Subscription costs are 'significant'.... however many libraries still have the older ASMH on shelves [or on-line].
In real terms the ASMD [ASMH] along with MMPDS... would replace a corporate-developed metals database/design handbook series with highly authoritative data recognized by the FAA and DoD.... assuming industry standards and practices for aerospace metals specifications and basic heat treatments, etc.
CINDAS
1501 = ASMH designation for 17-4PH CRES, all forms.
other examples...
1309 = 347 & 348 CRES [all forms]
3203 = 2024 aluminum bare/wrought products
3222 = 7050 aluminum [all]
3505 = HM31A magnesium [all]
4103 = Inconel 718
Etc.
Regards, Wil Taylor
o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]