Manufacturing processes such as chrome plating can have an adverse effect on both fatigue life and fatigue strength. Let's say you make the following statements:
1. The process may reduce the fatigue life of a component by 50%.
2. The process may reduce the fatigue strength of a component by 50%.
It's my understanding that a 50% reduction in fatigue strength is much worse than a 50 % reduction in fatigue life (i.e., a 50% reduction in fatigue strentgh can result in much more than a 50% reduction in fatigue life).
Can someone explain