Mar 5, 2003 #1 22west Mechanical Joined Oct 31, 2002 Messages 80 Location CA Does anyone have an S-N curve for 304 or else 304L?
Mar 5, 2003 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US There is a lot of information regarding fatigue in 304 stainless steel in ASM HANDBOOK Volume 19 Fatigue and Fracture, available at: http://www.asminternational.org Upvote 0 Downvote
There is a lot of information regarding fatigue in 304 stainless steel in ASM HANDBOOK Volume 19 Fatigue and Fracture, available at: http://www.asminternational.org
Mar 10, 2003 #3 Riadsala Materials Joined Feb 4, 2003 Messages 12 Location GB Otherwise try the Nickel Development Institute - they recently put a load of their data online! http://www.nidi.org Upvote 0 Downvote
Otherwise try the Nickel Development Institute - they recently put a load of their data online! http://www.nidi.org
Mar 10, 2003 Thread starter #4 22west Mechanical Joined Oct 31, 2002 Messages 80 Location CA Thanks alot, all this info was very helpful. http://www.nidi.org is a great site! Upvote 0 Downvote