Jul 6, 2018 #1 jtseng123 Mechanical Joined Jun 6, 2012 Messages 530 Location US Dear all, We have a high strength vessel, UTS is between 86 ksi-93 ksi in cyclic service. But Div 2, Fig 3-F does not have a curve for such UTS. Where can I find one ?
Dear all, We have a high strength vessel, UTS is between 86 ksi-93 ksi in cyclic service. But Div 2, Fig 3-F does not have a curve for such UTS. Where can I find one ?
Jul 6, 2018 #2 TGS4 Mechanical Joined Nov 8, 2004 Messages 3,995 Location CA Per 3-F.1.2(a) ASME Section VIII said: ... The fatigue curve values may be interpolated for intermediate values of the ultimate tensile strength. Click to expand... Upvote 0 Downvote
Per 3-F.1.2(a) ASME Section VIII said: ... The fatigue curve values may be interpolated for intermediate values of the ultimate tensile strength. Click to expand...
Jul 6, 2018 Thread starter #3 jtseng123 Mechanical Joined Jun 6, 2012 Messages 530 Location US TGS4, thanks Upvote 0 Downvote