Hi,

Are certain fatigue criteria more relevant for certain type of materials? I heard that Gerber is good for ductile materials, etc. So can we use criterion based on material? Any particular reference on this?

Thank you
Geoff
 
> The following information are valid for high-cycle fatigue (S-N method):

For steels and metals in general, the best fatigue criteria are classified in this sequence:

1) Walker model
2) Morrow model
3) SWT model (Smith–Watson–Topper model)

For Aluminium and titanium alloys, the best fatigue criteria are classified in this sequence:

1) Walker model
2) SWT model
3) Morrow model

Source:
 