Aug 30, 2006 #1 giamma109 Mechanical Joined Aug 29, 2006 Messages 27 Location IT Dear Group, I just joined the group and I need information about fatigue behaviour of aluminium alloy 7050 and, if it is possible, about 8090 alloy. Thank you!
Dear Group, I just joined the group and I need information about fatigue behaviour of aluminium alloy 7050 and, if it is possible, about 8090 alloy. Thank you!
Aug 30, 2006 1 #2 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US Al 7050 properties (for T7351, T74, T7451, T7452 & T7651 tempers) are on pages 3-322 to 3-362 in MIL-HDBK-5J METALLIC MATERIALS AND ELEMENTS FOR AEROSPACE VEHICLE STRUCTURES (31-JAN-2003) available from ASSIST: http://assist.daps.dla.mil/quicksearch/basic_profile.cfm?ident_number=53876 Upvote 0 Downvote
Al 7050 properties (for T7351, T74, T7451, T7452 & T7651 tempers) are on pages 3-322 to 3-362 in MIL-HDBK-5J METALLIC MATERIALS AND ELEMENTS FOR AEROSPACE VEHICLE STRUCTURES (31-JAN-2003) available from ASSIST: http://assist.daps.dla.mil/quicksearch/basic_profile.cfm?ident_number=53876
Aug 30, 2006 Thread starter #3 giamma109 Mechanical Joined Aug 29, 2006 Messages 27 Location IT thaks!!! Upvote 0 Downvote
Aug 30, 2006 1 #4 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US Alcan Aerospace developed alloy 8090, so I would contact them for fatigue information. Here is their contact page on the Internet: http://www.alcanaerospace.com/Aerospace/aerospace.nsf/html/FWFGHOME?Open&LG=1 Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
Alcan Aerospace developed alloy 8090, so I would contact them for fatigue information. Here is their contact page on the Internet: http://www.alcanaerospace.com/Aerospace/aerospace.nsf/html/FWFGHOME?Open&LG=1 Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Aug 30, 2006 Thread starter #5 giamma109 Mechanical Joined Aug 29, 2006 Messages 27 Location IT thanks Cory!!! Upvote 0 Downvote