Mar 18, 2006 #1 sinerd Mechanical Joined Mar 18, 2006 Messages 1 Location US I was told you should not weld structual members in a fatige test facility, but have been not been given a reason. These are test facities for the testing of large articals such as aircraft. Thanks, L MOrton
I was told you should not weld structual members in a fatige test facility, but have been not been given a reason. These are test facities for the testing of large articals such as aircraft. Thanks, L MOrton
Mar 18, 2006 #2 Allen Mechanical Joined Feb 10, 2005 Messages 51 Location US Do you have any question? Upvote 0 Downvote
Mar 20, 2006 #3 rb1957 Aerospace Joined Apr 15, 2005 Messages 16,145 Location CA from my experience with test facilities, i'davoid welding the rig together out of concern for how the rig will deform. i'd bolt the thing together. Upvote 0 Downvote
from my experience with test facilities, i'davoid welding the rig together out of concern for how the rig will deform. i'd bolt the thing together.