Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Fastener Fatigue Analysis

Status
Not open for further replies.

boo1

Mechanical
Oct 31, 2001
2,129
Does any one have a detailed fastener analysis or report I could use for a guide?
 
Replies continue below

Recommended for you

Try the ASM Metals Handbook volume 11 "Failure Analysis and Prevention".

Good Luck
 
Machinery's handbook has a section on bolt torque, tension, and fatigue - - however, my copy (25th Edidtion) appears to have some small error(s) of some sort.
If you use the numbers you get from the Torquing guide there, but make the units ft-lbs, rather than the inch-lbs it says, you will be pretty close to standard guides.

Otherwise, here's a quick guide:
n is expected number of cycles
if n>1,000,000 use n=1,000,000

For Grade 5 Bolts: D = 1/4'' - 1-1/4''
T = [ 1 - (log(n))/30)*10^(3.95 + 3.145log(D) )

For Grade 5 Bolts: D = 1-3/8'' - 2-1/2''
T = [ 1 - (log(n))/30)*10^(3.96 + 3.07log(D) )


For Grade 8 Bolts: D = 1/4'' - 1-1/4''
T = [ 1.25 - (log(n))/24)*10^(3.95 + 3.145log(D) )

For Grade 8 Bolts: D = 1-3/8'' - 2-1/2''
T = [ 1.25 - (log(n))/24)*10^(3.96 + 3.07log(D) )

Hope this helps