Hello Friends,
I am struggling to correlate FEA results with experimental results. I work on polymer parts reinforced with glass fibers. I have stress strain curves for the material till failure. My FEA results are 50% off from the experimental results. The model is setup correctly.
I think my biggest problem is deciding a failure criteria within the software. I don’t know how to come up with a criteria that will decide the load at failure. Do I look at the load when the 1st element reaches the Ultimate Tensile Strength of the material? Or do I look at the load at which a certain percentage (say 15%) of elements cross the Ultimate Tensile Strength of the material. I want to know
1.How you decide based on the FEA results whether the part will fail or not?
2.How much correlation have you got when dealing with polymer parts reinforced with glass fibers?
3.What is the industry practice that works best?
Thanks
Anup
I am struggling to correlate FEA results with experimental results. I work on polymer parts reinforced with glass fibers. I have stress strain curves for the material till failure. My FEA results are 50% off from the experimental results. The model is setup correctly.
I think my biggest problem is deciding a failure criteria within the software. I don’t know how to come up with a criteria that will decide the load at failure. Do I look at the load when the 1st element reaches the Ultimate Tensile Strength of the material? Or do I look at the load at which a certain percentage (say 15%) of elements cross the Ultimate Tensile Strength of the material. I want to know
1.How you decide based on the FEA results whether the part will fail or not?
2.How much correlation have you got when dealing with polymer parts reinforced with glass fibers?
3.What is the industry practice that works best?
Thanks
Anup