MegaStructures
Structural
Are there rules of thumb for specified lengths of hot-rolled steel beams considering fabrication quality?
There's a conversation in the office whether a W10x45 can be rolled in one 30ft piece, or if it needs to be split and spliced in the field to avoid warping from the mill. My hunch is that this shape would be just fine to be milled at this length, but I am curious if there are certain rules of thumb that other offices follow for this. I do know all members should be limited under 40ft to allow for transportation on the main roadways without special permitting.
Thanks
There's a conversation in the office whether a W10x45 can be rolled in one 30ft piece, or if it needs to be split and spliced in the field to avoid warping from the mill. My hunch is that this shape would be just fine to be milled at this length, but I am curious if there are certain rules of thumb that other offices follow for this. I do know all members should be limited under 40ft to allow for transportation on the main roadways without special permitting.
Thanks