sarclee

Mechanical
Jan 14, 2022
105
Hi, I compared the stacking sequence between unitape and fabric in the picture... It looks the same in terms of number of plies...my understanding about fabric is woven bidirectional fibers, if it is (0)ply, it means 0/90 in one ply;if it is (45),it means +/-45 in one ply.

But the table seems 0/90 for fabric is for two plies...

Screenshot_20220530_080635_com.adobe.reader_edit_62445939106616_pkoaub.jpg
 
Replies continue below

Recommended for you

Isn't it warp and fill directions giving similar properties? Is there any significant impact with 0 warp or 90 warp?

Thank you so much!
 
In many fabrics the warp and weft properties are perfectly balanced. In real life, there are some systematic, non-random differences in any given roll of material. To get the best uniformity in laminate properties, it would best to alternate warp direction in x and y directions. This can start to get complicated, however. Particularly, if you are using satin weave fabrics where there is also a warp face and a weft face to consider, as well.
 
Looks like the headings and tables are mismatched.
 
My mistake, it was too early in the morning.
 