Apr 13, 2007 #1 rotaryguy Mechanical Joined Jul 13, 2006 Messages 39 Location US Hi guys, FA-20 alloy normally used as pump material for corrosive service. can anybody tell me FA-20 chemical properties and composition. Thanks
Hi guys, FA-20 alloy normally used as pump material for corrosive service. can anybody tell me FA-20 chemical properties and composition. Thanks
Apr 13, 2007 #2 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US Maybe a cross between Haynes' Ferralium® & Carpenter's Alloy 20™? Ferralium®255: Ni 5, Cr 25, Mo 3, Cu 2, Mn 1.5 Carpenter 20™: Ni 34, Cr 20, Mo 2.5, Cu 3.5, Cb 8 x C Upvote 0 Downvote
Maybe a cross between Haynes' Ferralium® & Carpenter's Alloy 20™? Ferralium®255: Ni 5, Cr 25, Mo 3, Cu 2, Mn 1.5 Carpenter 20™: Ni 34, Cr 20, Mo 2.5, Cu 3.5, Cb 8 x C
Apr 16, 2007 Thread starter #3 rotaryguy Mechanical Joined Jul 13, 2006 Messages 39 Location US thanks Ken it is Carpenter's Alloy. Upvote 0 Downvote
Apr 16, 2007 #4 EdStainless Materials Joined May 20, 2004 Messages 16,367 Location Waukesha WI USA It is a cast version of alloy 20. The UNS is N08007 (CN-7M). Many people assign there own names, even if they don't modify the chemistry. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
It is a cast version of alloy 20. The UNS is N08007 (CN-7M). Many people assign there own names, even if they don't modify the chemistry. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm