What is meant by the GP1 designation?

Ground and Polish?

Any info would be great.

cheers.

Rob.
 
Replies continue below

Recommended for you

If this is ASTM F593 Standard Specification, the GP is probably Group 1 designation.
 
Yes it is the ASTM F593 Standard Specification.
 
Group 1, which includes alloys 303, 304, 305, 384, XM1, and XM7.
 