I am proposing a WPS to qualify a plate test coupon with E316L electrode which comes under SFA-5.4 per SEC II PART C.
What will be the F Number for the same?
Per me its F5 per QW 432 of SEC IX but our existing old wps shows F4,so i am little bit confuse.
 
It is F5. How old is your old procedure? It could have been a typographical error, which was never corrected.

 
you r right. It must be a mistake which never got corrected.
now i will take care in the current WPS. thanks.
 