Hello everbody,
During my researchs, DIN and EN standarts making lots of trouble to me about heat treatment processes, and wasting my time.
They're so confusing because of their differences. According to DIN standarts heat treatment at 6063 F22, 6063 F25 and in EN standarts 6063 T6, 6063 T66 etc etc..
And also, 6005 alloy heat treatment in DIN standarts is different from 6063 DIN standarts. I mean they're not symbolises same process and hardness for every alloy. (Even if, 6005 F22 - 6063 F22). Last of all, for example what 22 tells us in F22?
In conclusion, is there any table or software (?) that's gonna help me with this problem. Maybe a website ?
During my researchs, DIN and EN standarts making lots of trouble to me about heat treatment processes, and wasting my time.
They're so confusing because of their differences. According to DIN standarts heat treatment at 6063 F22, 6063 F25 and in EN standarts 6063 T6, 6063 T66 etc etc..
And also, 6005 alloy heat treatment in DIN standarts is different from 6063 DIN standarts. I mean they're not symbolises same process and hardness for every alloy. (Even if, 6005 F22 - 6063 F22). Last of all, for example what 22 tells us in F22?
In conclusion, is there any table or software (?) that's gonna help me with this problem. Maybe a website ?