Hi Everyone, Does anyone have any mechanical properties (UTS, yield,elongation) for 7129 aluminum alloy as it applies to extrusions? The higher T tempers are what I would be interested in. My references are not new enough to have it, and I'm not having a lot of luck finding it on the internet. Thanks.
 
T5,T6 typical:
430 MPa UTS
380 MPa YS
15% El
270 MPa Shearing Strength
-Alcoa 1987
 