MatEngTED

Materials
Sep 27, 2004
24
Looking for a polymer to extrude over a metal coil. Material must be gamma sterilizable to 90 kGy, Coil is approximately 10 ft. long and 0.1 in. in diameter. Material must be low cost.
 
Replies continue below

Recommended for you

Try thermoplastic Polyurethane, for example Desmopan from Bayer. They have medical grades with may be irradiated.
 