For P-No. 1 Group Nos. 1 and 2 materials the extreme
fiber elongation may be as great as 40% when none
of the conditions listed below in (1) through (5) exist.
(1) The vessel will contain lethal substances either
liquid or gaseous (see UW-2).
(2) The material requires impact testing.
(3) The thickness of the part before cold forming
exceeds 5?8 in. (16 mm).
(4) The reduction by cold forming from the as rolled
thickness is more than 10%.
(5) The temperature of the material during forming
is in the range of 250°F to 900°F (121°C to 482°C).
I would like to know about item No.4. how to check and how to calculation?
thank you all for kindly
fiber elongation may be as great as 40% when none
of the conditions listed below in (1) through (5) exist.
(1) The vessel will contain lethal substances either
liquid or gaseous (see UW-2).
(2) The material requires impact testing.
(3) The thickness of the part before cold forming
exceeds 5?8 in. (16 mm).
(4) The reduction by cold forming from the as rolled
thickness is more than 10%.
(5) The temperature of the material during forming
is in the range of 250°F to 900°F (121°C to 482°C).
I would like to know about item No.4. how to check and how to calculation?