yamoffathoo
Mechanical
- Sep 19, 2008
- 87
1978 TEMA C recommended that for 300 psig+ and 350 degF + heat exchangers with 5/8" dia and larger tubes you should either expand the tubes over 1-1/4" min. length in a two-grooved tubesheet or use full strength seal welds.
If the 5/8" dia tubes are presently rolled 3" long in a 6" thick tubesheet without grooves and SSC has cracked through the tubes next to the seal welds, is there a case for expanding the 3" un-rolled section rather than re-welding the seal weld?
If the 5/8" dia tubes are presently rolled 3" long in a 6" thick tubesheet without grooves and SSC has cracked through the tubes next to the seal welds, is there a case for expanding the 3" un-rolled section rather than re-welding the seal weld?