Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Expansion Joint vs flexible joint

Status
Not open for further replies.

Dj364

Mechanical
Jun 24, 2007
35
Dear Members,
Could any one has a thought about using flexible joint instead of expasion joint?
I'll appreciate your feedback.
Regards.
Dj364
 
Replies continue below

Recommended for you

Dj364
What is the line size(es)
What is the product in the line?
What is the pressure?
What is the temperature?
What is the pipe material?
 
Yes , thanks for your reply...
line size is 10", DesP 0.18 bar (2.6 psi), DesT=110 C (230F), pipe material Stainless steel (304/304L).
Thanks in advance,
Dj364
 
Ideally a solid pipe is best where reliabilty and degredation issues can be dealt with,saying that if it was required to flex or move with a load or other device a flexible joint would be my prefered choice, depending on fluid,application,pressure and immediate environment
 
expansion joints are preferred for SLIGHT lateral, axial, and angular motions or vibration isolation. Hoses can do the same except with not allowable axial movements. At 230 F, you may want PTFE over the elastomers.
 
in our case the client prefers to have flexible hose connection instead of expansion joint.
But flexible hose connot be modeled in caesar II programm ( beam thoery).
so I am mdeling at the point location as free end , with Axial anchor close and limit the operating lateral mvt to 3mm, and axial operating mvt 5 mm.
is it a good approach?
I will appreciate you do have other tips for modeling the flexible hose.
Thanks'
Dj364
 
You will certainly shorten the expected life of a flexible hose if it will be expected to contract/expand axially. If you design the hose as a loop, so that axial movement opens/closes the loop, you can expect much better life.
 