Has anyone used DME's "Expandable Cavity System" to mold Nylon? Does the cavity clamp tight enough to prevent flash? Does it produce large witness lines? Any help on this would be great. Thanks
 
Replies continue below

Recommended for you

A cursory Google search revealed no precise info, apart from "Contact DME for info".

On that basis I would have reservations.

Ask DME for customers who use it and give them a call (their customers, that is)...I bet a pound to a pinch of s**t they won't give you any phone numbers!