Dear all,
I am reviewing my Vendor's WPS and looking to your advice.
I understand that ASME VIII-Div1 UCS 56 table exempts from PWHT for SA537 Cl2 of 38mm & below thickness.
The Vendor's PQR passed all mechanical tests (impact test at -48C) and both tensile specimens broke at weld metal. The PQR weld is obviously weaker than Base Metal taking into account that SA537 Cl2 is the Quenched and Tempered steel (at 910C & 610C accordingly by steel maker).
Thus, please consult me if the design concept of making weld weaker than Base Metal is considered as the optimization in engineering view.
Thanks a lot.
I am reviewing my Vendor's WPS and looking to your advice.
I understand that ASME VIII-Div1 UCS 56 table exempts from PWHT for SA537 Cl2 of 38mm & below thickness.
The Vendor's PQR passed all mechanical tests (impact test at -48C) and both tensile specimens broke at weld metal. The PQR weld is obviously weaker than Base Metal taking into account that SA537 Cl2 is the Quenched and Tempered steel (at 910C & 610C accordingly by steel maker).
Thus, please consult me if the design concept of making weld weaker than Base Metal is considered as the optimization in engineering view.