What are european standards that I have to specify for ordering the following structural steel shapes:
- Channel
- I beam
- Standard beam
- Wide flange beam
- Hollow structural steel
 
You can perform a keyword search for various standards (BS, EN, ISO, etc.) at Global Engineering's website:

 
Try looking at BS EN 10025 and BS EN 10210. These specifications have been broken out from the now obsolete BS 4360.
 