Jan 10, 2003 #1 vitathedog Mechanical Joined Jan 10, 2003 Messages 6 Location CA What is european standard that I have to use to specify (order) steel plate? EN 10027 or 10025?
Jan 10, 2003 1 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US EN 10025 governs flat products such as sheet, strip, and plate. It references EN 10027 which lists chemical compositions for various steel grades. You should use EN 10025 when specifying plate for your application. Upvote 0 Downvote
EN 10025 governs flat products such as sheet, strip, and plate. It references EN 10027 which lists chemical compositions for various steel grades. You should use EN 10025 when specifying plate for your application.
Jan 13, 2003 1 #3 ijzer Materials Joined Oct 25, 2002 Messages 313 Location NL To be more precise: EN 10025 for plate for non-pressure parts EN 10028 for plate for pressure parts Upvote 0 Downvote