Dear All,
I want to model the metal particle impact (at high velocity) on to a metal substrate (cold spray process).
Due to excessive deformation I have to use Eulerian method.
So I would like to know how should I make this model. I did as bellow but my model is not working!
I defined the parts: one Eulerian part, and two 3D-deformable parts as substrate and particle.
Then I assigned material: I defined an Eulerian section and assigned that to Eulerian part and then defined a Solid-Homogeneous section and assigned that to 3D-and deformable parts (substrate and particle).
At Interaction module: I defined general contact--> "all with self" with "Tangential and Normal behavior" interaction property. And two Discrete fields (Volume fraction tool) to fill particle and substrate with Eulerian material.
At load module: I defined velocity for the particle.
I also meshed all parts.
As I tolled the model was not successful. I changed many thing but still not succeed.
Could anyone help me? I really appreciate.
BW,
Zohreh
I want to model the metal particle impact (at high velocity) on to a metal substrate (cold spray process).
Due to excessive deformation I have to use Eulerian method.
So I would like to know how should I make this model. I did as bellow but my model is not working!
I defined the parts: one Eulerian part, and two 3D-deformable parts as substrate and particle.
Then I assigned material: I defined an Eulerian section and assigned that to Eulerian part and then defined a Solid-Homogeneous section and assigned that to 3D-and deformable parts (substrate and particle).
At Interaction module: I defined general contact--> "all with self" with "Tangential and Normal behavior" interaction property. And two Discrete fields (Volume fraction tool) to fill particle and substrate with Eulerian material.
At load module: I defined velocity for the particle.
I also meshed all parts.
As I tolled the model was not successful. I changed many thing but still not succeed.
Could anyone help me? I really appreciate.
BW,
Zohreh