May i know the best etching agent for composite material microstructure study.

Thanks
 
What materials? What features are you trying to see?
I always start with no etch. Try DIC and pol lighting to see features. If I need more I try heat tinting. Then I use etchants.

= = = = = = = = = = = = = = = = = = = =