I have a drawing note that says: ETA Phase to be .004" Maximum. this is for a forging which is supplied in the heat treated condition RC 32-38. Based on my limited knowledge of this phase I will assume like all metallurgy this phase is developed during the forging temperature and operation and then enhanced during the heat treatment cycle?
I do have limits on my max. forging temps, so I will also assume (bad word) that the lowest temp I can get away with forging the better off I will be.
Are these logical assumptions?
Thanks
John
I do have limits on my max. forging temps, so I will also assume (bad word) that the lowest temp I can get away with forging the better off I will be.
Are these logical assumptions?
Thanks
John