Hello.
What is the basic steps of estimating rate of corrosion for piping runs?
Assuming uniform corrosion and erosion.
The fluid contains following in mg/kg:
CO2: 56,7
H2S: 85,3
SiO2: 694,8
Na: 152,2
SO4: 18,9
other parameters:
Temp: 210 degree Cecius
Velocity: 40m/s
Is there a way I can estimate the corrosion rate? i'm designing a pipe run that must have life span of 25years and preferebly I want to use Carbon steel. I am designing in accordance with ASME B31.3
What is the basic steps of estimating rate of corrosion for piping runs?
Assuming uniform corrosion and erosion.
The fluid contains following in mg/kg:
CO2: 56,7
H2S: 85,3
SiO2: 694,8
Na: 152,2
SO4: 18,9
other parameters:
Temp: 210 degree Cecius
Velocity: 40m/s
Is there a way I can estimate the corrosion rate? i'm designing a pipe run that must have life span of 25years and preferebly I want to use Carbon steel. I am designing in accordance with ASME B31.3