anyone know of research or had experience of the following.
C60 concrete, incl 20kgs m/silica supplied to a project. Cubes at 7 days 55-60kn so no problem there. Client is unhappy with workmanship and wants to know strength of insitu concrete. Cores drilled at 9 days, these will be crushed at 14 days. Little or no curing on site
What strength should we expect from these cores ?
C60 concrete, incl 20kgs m/silica supplied to a project. Cubes at 7 days 55-60kn so no problem there. Client is unhappy with workmanship and wants to know strength of insitu concrete. Cores drilled at 9 days, these will be crushed at 14 days. Little or no curing on site