Hello I am brand new to this forum so if this question has been answered elsewhere just point me in the right direction.
I currently have a procedure that is qualified with EM12K and want to know if I can now use an EM13K wire without requalifying. In detail I would like to go from an F7A4-EM12K-H8 to an F7A4-EM13K-H8. My interpretation is that I can because I am not changing the material group or classification. Working to AWS D1.1 code.
 
Replies continue below

Recommended for you

What welding standard are you working with. Different codes, different variables.

Best regards - Al
 
No, I just need to clean my glasses more frequently.

How's the world treating you lad?

Since you stated the WPS is qualified, I assume it was qualified in accordance with Clause 4, because it didn't meet the conditions of prequalification or notch toughness is a requirement for your application.

If the WPS is qualified in accordance with AWS D1.1:2010, clause 4, any change in the flux / electrode classification requires requalification. Please refer to Table 4.5, item 3. Look to Table 4.6 if notch toughness is a requirement.