Hello everyone,
Problem : Frequent failure of 8" SS304L pipe line due to the slurry erosion.The pipeline faces a vertical ( top to bottom) flow and the isometrics of the pipe has two elbows 30 and 45 degree. The erosion mainly takes place the hitting edges of these elbow outlet regions.
Process media : petcoke slurry; temperature will be around 70-80 degree Celsius ; it contains chlorides and little H2S. velocity may be around 15- 20 m/s
The erosion mainly takes place in the extra-dose of the elbow and bottom side of the slant pipe line ( sliding abrasion)
Immediate action taken : conforma clad. this gave as temporary relief of about 6-7 months breathing time.
i am here looking for extended life of these lines. I have searched and found few possible solutions as enlisted below,
1. High manganese Steel- Better impact resistance and work hardens. But it lacks sliding abrasion resistance
2. UHMWPE pipes - Heard these have good properties to meet my requirement. But does this handle pressure ? Any experience comments and thoughts required please
3. Basalt lining - Good sliding abrasion ; but Impact resistance ???
i would like to hear more about solution of my problem
thanks in advance.
Problem : Frequent failure of 8" SS304L pipe line due to the slurry erosion.The pipeline faces a vertical ( top to bottom) flow and the isometrics of the pipe has two elbows 30 and 45 degree. The erosion mainly takes place the hitting edges of these elbow outlet regions.
Process media : petcoke slurry; temperature will be around 70-80 degree Celsius ; it contains chlorides and little H2S. velocity may be around 15- 20 m/s
The erosion mainly takes place in the extra-dose of the elbow and bottom side of the slant pipe line ( sliding abrasion)
Immediate action taken : conforma clad. this gave as temporary relief of about 6-7 months breathing time.
i am here looking for extended life of these lines. I have searched and found few possible solutions as enlisted below,
1. High manganese Steel- Better impact resistance and work hardens. But it lacks sliding abrasion resistance
2. UHMWPE pipes - Heard these have good properties to meet my requirement. But does this handle pressure ? Any experience comments and thoughts required please
3. Basalt lining - Good sliding abrasion ; but Impact resistance ???
i would like to hear more about solution of my problem
thanks in advance.