ER80S-Ni1

Status
Not open for further replies.

ZHA

Materials
Joined
Aug 10, 2017
Messages
60
Location
US
Is post heating (at 300 C for 2 hours) necessary for ER80SNi1 weld consumable for API 5L X65 Pipe?
 
No, as long as proper preheat and good cleanliness are used.
 