May 3, 2005 #1 weldtek Materials Joined Feb 12, 2005 Messages 897 Location US Anyone know of a supplier in the US?
May 3, 2005 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US weldtek; Try Boehler-Thyssen. They have a distribution center in the US. We have purchased from them - excellent people to deal with and great products. The SFA 5.9 ER410 NiMo SAW wire is supplied by B-T, and is Thermanit 13/04, Mat No 1.4351. http://www.btwcan.com/html/product_lines.html Upvote 0 Downvote
weldtek; Try Boehler-Thyssen. They have a distribution center in the US. We have purchased from them - excellent people to deal with and great products. The SFA 5.9 ER410 NiMo SAW wire is supplied by B-T, and is Thermanit 13/04, Mat No 1.4351. http://www.btwcan.com/html/product_lines.html
May 4, 2005 #3 GRoberts Materials Joined Apr 22, 2002 Messages 548 Location US Try Techalloy http://www.techalloy.com/Weld Techalloy Data Sheets/TECHALLOY 410NiMo.pdf Upvote 0 Downvote