As per welding schedule ER 70S-A1 Filler wire was to be used for welding Carbon steel joints of Boiler tubes, But the contractor by mistake used ER-70S2 filler for some joints. Will this have adverse effect on performance of boiler ? do we need to cut entire joints..?? What can be the possible adverse effect if we don't cut such joints..?

Pls. help

Alok
 
Replies continue below

Recommended for you

Life of welds would depend on operating temperature. ER70S-2 has been used on carbon steel tubes for decades and is stiil be used for boiler tubes.
 