Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Equivalent Stress at root of Fillet Weld for fatigue assessment (Nozzle Re-Pad)

Status
Not open for further replies.

MrPDes

Mechanical
Joined
Jun 18, 2013
Messages
96
Location
GB
I have an Ellipsoidal Head with a nozzle in its centre. The nozzle has a Reinforcing Pad with a fillet weld around its outside diameter.

The "effective alternating equivalent" stress at the root of this outer fillet weld is needed (in accordance with Step 3 of 5.5.3.2 of ASME VIII Div 2.), so that it can be assessed for fatigue.

Shall this stress be calculated using the "Effective Notch Stress Method" shown on Slide 10 of the following link? Is this method compatible with ASME VIII Div 2?

As the stress taken from the FEA does not include the notch effect, Step 4(a) of 5.5.3.2 of ASME VIII Div 2 would then require that Kf = 4.0 for the root of the weld (from Table 5.11).

The shell and head thickness are both 22mm thick. Material: SA-516 Gr70.