May 24, 2002 #1 pardal Automotive Joined Oct 17, 2001 Messages 444 Location AR I had done an aproach to my need abbout steel DO04 under FN EN 10130 It is a DIN 1623 ST 14 or BS 1449 CR 1 please give me a equivalent to AISI. Thanks again Pardal
I had done an aproach to my need abbout steel DO04 under FN EN 10130 It is a DIN 1623 ST 14 or BS 1449 CR 1 please give me a equivalent to AISI. Thanks again Pardal
May 30, 2002 #2 evmundo Automotive Joined May 30, 2002 Messages 8 Location GB Try http://www.matweb.com/GetKeywordMatls.asp for all AISI materials Upvote 0 Downvote
May 30, 2002 Thread starter #3 pardal Automotive Joined Oct 17, 2001 Messages 444 Location AR I had found it . It is a AISI 1006 cold draw steel, low carbon < 0.08% C Pardal Upvote 0 Downvote