Equivalent of SA 335 Gr.P1 1

Status
Not open for further replies.

ReTube

Materials
Jul 22, 2012
10
Hi,
will somebody please let me know what Equivalent or Alternate material of SA 335 Gr.P1, I need
Equivalent = BS/EN
Equivalent = DIN
Alternate within ASME.
( Thanks in advance )
 
Replies continue below

Recommended for you

Within ASME material specifications,
SA 369 FP1 could be used as an alternate to SA 335 Gr P1. In fact, this material can be dual certified between the two material specifications.
 
The closest EN equivalent would be:

16Mo3 per EN 10216-2
 